Tembaga Nikel Kobalt Beryllium Alloy Rod lan Kawat (CuNiBe C17510)
1. Komposisi Kimia C17510
Model | Be | Co | Ni | Fe | Al | Si | Cu |
C17510 | 0.2-0.6 | ≤0.3 | 1.4-2.2 | ≤0.1 | ≤0.20 | ≤0.20 | Turahan |
2. Sifat Fisik lan Mekanik C17510
negara | Kinerja | |||
Kode Standar | Babagan | Kekuwatan Tarik (MPa) | Kekerasan (HRB) | Konduktivitas Listrik (IACS,%) |
TB00 | Perawatan Solusi Padat (A) | 240-380 | Min50 | 20 |
TD04 | Perawatan Solusi Padat & Proses Pengerasan Dingin (H) | 450-550 | 60-80 | 20 |
| Sawise Perawatan Panas Deposit | |||
TF00 | Heat Treatment Of Deposit (AT) | 690-895 | 92-100 | 45 |
TH04 | Hardening & Deposit Heat Treatment of Settlement(HT) | 760-965 | 95-102 | 48 |
3. Bidang Aplikasi saka C17510
Utamane digunakake kanggo welding, tumpukan pangisi daya mobil anyar lan industri komunikasi